Durethan@ BG 30 x000000 (干燥) PA6.30 %玻璃纤维/玻璃球,注塑成型,低倾向于翘曲和杜乙烷BG 30X 00000 PA 6。30%玻璃纤维/alass球。注塑成型,低翘曲倾向 Durethan? BG30X 000000 (Dry) PA 6, 30 % glass fibers/glass spheres, injection molding, low tendency to warp Durethan? BG30X 000000 PA 6, 30 % glass fibers/glass spheres, injection molding, low tendency to warp Durethan? BG30X 000000 PA 6, 30 % glass fibers/glass spheres, injection molding, low tendency to warp |
技术参数Technical Data | |||
---|---|---|---|
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
密度Specific Gravity | 1.35 | g/cm3 | ASTM D792 |
密度Density (73°F) | 1.35 | g/cm3 | ISO 1183 |
表观密度Apparent Density | 0.70 | g/cm3 | ISO 60 |
收缩率Molding Shrinkage | ISO 294-4 | ||
TD:280℃,2.0 mmAcross Flow : 536°F, 0.0787 in 22 | 0.77 | % | ISO 294-4 |
TD:120℃,2.0 mm,2 hrsAcross Flow : 120°C, 2 hr, 2.00 mm 33 | 0.16 | % | ISO 294-4 |
MD:280℃,2.0 mmFlow : 536°F, 0.0787 in 22 | 0.48 | % | ISO 294-4 |
MD:120℃,2.0 mm,2 hrsFlow : 120°C, 2 hr, 2.00 mm 33 | 0.12 | % | ISO 294-4 |
吸水率吸水率 | |||
饱和,23℃饱和,23℃ | 7.0 | % | ISO 62 |
平衡,23℃,50% RH平衡,23℃,50% RH | 2.2 | % | ISO 62 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
膜刺穿强度Film Puncture Energy | ISO 6603-2 | ||
---- 77 | 1.70 | J | ISO 6603-2 |
---- 88 | 2.00 | J | ISO 6603-2 |
膜刺穿力Film Puncture Force | ISO 6603-2 | ||
---- 77 | 690 | N | ISO 6603-2 |
---- 88 | 700 | N | ISO 6603-2 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
简支梁缺口冲击强度Charpy Notched Impact Strength | ISO 179/1eA | ||
-40℃-40°C | 10 | kJ/m2 | ISO 179/1eA |
-30℃-30°C | 10 | kJ/m2 | ISO 179/1eA |
23℃23°C | 10 | kJ/m2 | ISO 179/1eA |
简支梁无缺口冲击强度Charpy Unnotched Impact Strength | ISO 179/1eU | ||
-30℃-30°C | 40 | kJ/m2 | ISO 179/1eU |
23℃23°C | 45 | kJ/m2 | ISO 179/1eU |
悬臂梁缺口冲击强度Notched Izod Impact Strength | ASTM D256 | ||
-40℃,3.2mm-40°C, 3.18 mm | 48 | J/m | ASTM D256 |
23℃,3.2mm23°C, 3.18 mm | 59 | J/m | ASTM D256 |
悬臂梁缺口冲击强度Notched Izod Impact Strength | ISO 180/1A | ||
-40℃-40°C | 10 | kJ/m2 | ISO 180-1A |
-30℃-30°C | 10 | kJ/m2 | ISO 180-1A |
悬臂梁无缺口冲击强度Unnotched Izod Impact Strength | ISO 180/1U | ||
-30℃-30°C | 30 | kJ/m2 | ISO 180/1U |
23℃23°C | 35 | kJ/m2 | ISO 180/1U |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
热变形温度热变形温度 | |||
1.8 MPa,未退火,4.0 mm1.8 MPa,未退火,4.00 mm | 180 | ℃ | ASTM D648 |
1.8 MPa,未退火1.8 MPa,未退火 | 190 | ℃ | ISO 75-2/A |
0.45 MPa,未退火,4.0 mm0.45 MPa,未退火,4.00 mm | 200 | ℃ | ASTM D648 |
0.45 MPa,未退火0.45 MPa,未退火 | 210 | ℃ | ISO 75-2/B |
维卡软化温度Vicat Softening Temperature | |||
B50-- | 200 | ℃ | ISO 306 |
B120-- | 200 | ℃ | ISO 306/B120 |
熔融温度Melting Temperature 55 | 222 | ℃ | ISO 11357-3 |
线性热膨胀系数线性热膨胀系数 | |||
TD:23~55℃TD:23 到 55℃ | 9.0E-5 | 1/℃ | ISO 11359-2 |
MD:23~55℃MD:23 到 55℃ | 3.0E-5 | 1/℃ | ISO 11359-2 |
相对温度指数相对温度指数 | |||
电气性能,1.50 mm电气性能,1.5 mm | 120 | ℃ | UL 746 |
强度机械性能,1.50 mm强度机械性能,1.5 mm | 125 | ℃ | UL 746 |
冲击机械性能,1.50 mm冲击机械性能,1.5 mm | 90.0 | ℃ | UL 746 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
表面电阻率Surface Resistivity | 1.0E+14 to 1.0E+16 | ohms | IEC 60093 |
体积电阻率体积电阻率 | |||
23℃23℃ | 1.0E+15 | ohms·cm | IEC 60093 |
介电强度Electric Strength | IEC 60243-1 | ||
23 ℃,1 mm23°C, 1.00 mm | 36 | kV/mm | IEC 60243-1 |
23 ℃,3 mm23°C, 3.00 mm | 35 | kV/mm | IEC 60243-1 |
介电常数Dielectric Constant 1010 | IEC 60250 | ||
23 ℃,50 Hz23°C, 50 Hz | 4.50 | IEC 60250 | |
23 ℃,1 MHz23°C, 1 MHz | 4.00 | IEC 60250 | |
相对电容率Relative Permittivity | IEC 60250 | ||
23℃,100 Hz23°C, 100 Hz | 4.50 | IEC 60250 | |
23℃,1 MHz23°C, 1 MHz | 4.00 | IEC 60250 | |
耗散因数Dissipation Factor | IEC 60250 | ||
23℃,50 Hz23°C, 50 Hz | 0.015 | IEC 60250 | |
23℃,100 Hz23°C, 100 Hz | 0.013 | IEC 60250 | |
23℃,1 MHz23°C, 1 MHz | 0.020 0.018 | IEC 60250 | |
耐电弧性Arc Resistance | -- | sec | ASTM D495 |
相比漏电起痕指数Comparative Tracking Index | -- | V | ASTM D3638 |
解决方案 A解决方案 A | 400 | V | IEC 60112 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
阻燃等级Flame Rating | UL 94 | ||
1.50 mm1.5 mm | HB | UL 94 | |
1.60 mm1.6 mm | HB | UL 94 | |
3.00 mm3.0 mm | HB | UL 94 | |
3.20 mm3.2 mm | HB | UL 94 | |
灼热丝可燃性指数灼热丝可燃性指数 | |||
2.0 mm2.0 mm | 650 | ℃ | IEC 60695-2-12 |
极限氧指数Oxygen Index 1111 | 23 | % | ISO 4589-2 |
阻燃等级Burning Behavior 1212 | passed | ISO 3795 | |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
ISO ShortnameISO Shortname | PA 6, GR, 14-060, (GB+GF) 30 | ISO 1874 | |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
拉伸模量拉伸模量4 | |||
23℃23℃ | 6300 | MPa | ISO 527-1-2 |
23℃23℃4 | 6200 | MPa | ASTM D638 |
拉伸强度拉伸强度 | |||
断裂,23℃断裂,23℃ | 125 | MPa | ISO 527-2/5 |
断裂,23℃断裂,23℃ | 125 | MPa | ASTM D638 |
拉伸应变拉伸应变 | |||
断裂,23℃断裂,23℃ | 4.0 | % | ISO 527-2/5 |
断裂,23℃断裂,23℃ | 4.0 | % | ASTM D638 |
Tensile Creep Modulus(1 hr)Tensile Creep Modulus (1 hr) | -- | MPa | ISO 899-1 |
拉伸蠕变模量拉伸蠕变模量 | |||
1000 hr1000 hr | -- | MPa | ISO 899-1 |
弯曲模量弯曲模量5 | |||
23℃23℃ | 5500 | MPa | ASTM D790 |
23℃23℃5 | 5800 | MPa | ISO 178-A |
弯曲强度Flexural Stress 55 | |||
23℃23℃ | 195 | MPa | ASTM D790 |
3.50% 应变3.5% Strain | 170 | MPa | ISO 178-A |
23℃23°C | 185 | MPa | ISO 178 |
弯曲应变Flexural Strain at Flexural Strength 6 (23°C)6 | 5.0 | % | |
球压硬度Ball Indentation Hardness | 185 | MPa | ISO 2039-1 |
江苏普及塑料有限公司
联系人:
何志伟
服务热线:
존솓퍴존ꈗꁣꈗ솓
존솓퍴존ꈗꁣꈗ솓
公司地址:
陆家镇陆丰东路3号仕泰隆模具城M区511室
-
注塑级 PP利安德巴塞尔 HP525N 高清晰度 食品接触 易加工 高刚性¥0.01元
-
PP 韩国sk B391G 高抗冲共聚物 高流动 高刚性 食品级 40熔融指数¥0.01元
-
高流动PP 韩国sk/BX3920耐高温高抗冲高刚性注塑级¥0.01元
-
PP 韩国SK B380G 高流动 高抗冲 高光泽 用于家电部件 聚丙烯PP¥0.01元
-
PP韩国SK B330F尺寸稳定高抗撞抗冲共聚物高韧性电池盒电气/电子¥0.01元
-
注塑级 PP/韩国sk/B340F 高强度 高抗冲 共聚物 电子电器¥0.01元
-
PP台湾李长荣6331注塑颗粒低气味新料食品容器瓶盖均聚物塑胶原料¥0.01元
-
PP李长荣化工(福聚)PC366-3瓶盖料单聚合物高强度透明PP料PC366-4¥0.01元
德国朗盛PA6/BG30X 增强尼龙6 低翘曲性 加纤30% 高硬度注塑材料相关产品
- 专注PA6 玻纤增强30%德国巴斯夫B3W
- 供应PA6 易流动德国朗盛 B30S快速固化
- 供应 注塑 PA6 易流动德国朗盛 B30S PA6 易脱模 快速固化 PA6 尼龙进口塑料
- 专注 PA6 玻纤增强30%德国巴斯夫B3W PA6 尼龙进口塑料 PA6 玻纤增强
- 25%玻纤PA6 DOMAMID 6G25V0EF
- 25%玻纤PA6 DOMAMID 6G25
- 30%玻纤PA6 DOMAMID 6G30
- 30%玻纤PA6 DOMAMID 6G30GT96M
- 30%玻纤PA6 DOMAMID 6G30FC
- 20%玻纤PA6 DOMAMID 6G20GT96M
- PA6 DOMAMID 6G20V0EF
- 30%玻纤PA6 DOMAMID 6G30H
- 供应 防火PA6 广东新会美达 M2800本色耐高温,无卤增强塑料厂家批发价格
- 供应透明 YH800湖南岳化PA6尼龙中粘度塑料原料厂家直销
- 塑胶原料PA6台湾集盛TP-4208高熔子耐低温电子电器专用尼龙PA6纯树脂
- PA6价格塑料美国舒尔曼 6 GF15 流动性耐油性能尼龙塑料颗粒
- 黑色粒子PA6塑胶 美国舒尔曼 GF30润滑剂 导电性PA6塑料颗粒
- 注塑级尼龙塑胶PA6 美国舒尔曼 6MV14 FR4 K1681销售尼龙塑胶原料
猜你在找
- 机械设备PA6 荷兰DSM K224-PG3 阻燃级
- 专卖尼龙塑胶PA6荷兰DSM K224-HG6注塑级脱模级
- PA6 荷兰DSM K224-HG8 增强级
- PA6 阻燃增强级 K-FHGM24 注塑级
- PA6 电子计算机 K224-HG6 BK 注塑级
- 工程塑料PA6 工业零件2934A 注塑级塑料
- PA6 塑胶原料 K223-HGM24 工程塑料
- 热稳定性无卤阻燃性PA6 无卤阻燃性 K225-KS 耐热级
- PA6 工程塑料 K224-HG7 注塑级
- PA6塑料 K224-PG8 增韧级
- 尼龙PA6 荷兰DSM K224-HG6U注射成型33%玻纤增强PA6塑料
- 33%玻纤增强PA6 荷兰DSM K224-G6 注塑级
免责声明:以上展示的德国朗盛PA6/BG30X 增强尼龙6 低翘曲性 加纤30% 高硬度注塑材料信息由江苏普及塑料有限公司自行提供,内容的真实性、准确性和合法性由发布企业负责,
全球塑胶网对此不承担责任。
风险防范建议:为保障您的利益,建议优先选择速购通会员
手机版:德国朗盛PA6/BG30X 增强尼龙6 低翘曲性 加纤30% 高硬度注塑材料
更新产品链接为:https://www.51pla.com/html/sellinfo/486/48619089.htm
发送询价单