产品推荐
基本参数
牌号 | BKV30GH2.0 900051 | 厂商 | 德国朗盛 |
用途级别 | 通用级 | 销售方式 | 品牌经销 |
产品名称 | PA6 | 加工级别 | 注射级 |
形态 | 颗粒 | 批号 | 10+ |
类型 | 标准料 |
牌号简介About |
---|
Durethan? BKV 30 G H2.0 900051含有30%玻璃纤维增强的PA 6材料,用注射成型的方式进行加工,具有良好的热稳定性、表面光洁度以及耐候化性。 Durethan? BKV30GH2.0 900051 (Dry) PA 6, 30 % glass fibers, injection molding, heat-aging stabilized, improved surface finish, improved resistance to weathering Durethan? BKV30GH2.0 900051 PA 6, 30 % glass fibers, injection molding, heat-aging stabilized, improved surface finish, improved resistance to weathering Durethan? BKV30GH2.0 900051 PA 6, 30 % glass fibers, injection molding, heat-aging stabilized, improved surface finish, improved resistance to weathering |
技术参数Technical Data | |||
---|---|---|---|
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
密度Density (73°F) | 1.36 | g/cm3 | ISO 1183 |
表观密度Apparent Density | 0.70 | g/cm3 | ISO 60 |
收缩率Molding Shrinkage | ISO 294-4 | ||
TD:280℃,2.0 mmAcross Flow : 536°F, 0.0787 in 22 | 0.58 | % | ISO 294-4 |
TD:120℃,2.0 mm,2 hrsAcross Flow : 120°C, 2 hr, 2.00 mm 33 | 0.16 | % | ISO 294-4 |
MD:280℃,2.0 mmFlow : 536°F, 0.0787 in 22 | 0.27 | % | ISO 294-4 |
MD:120℃,2.0 mm,2 hrsFlow : 120°C, 2 hr, 2.00 mm 33 | 0.060 | % | ISO 294-4 |
吸水率吸水率 | |||
饱和,23℃饱和,23℃ | 6.5 | % | ISO 62 |
平衡,23℃,50% RH平衡,23℃,50% RH | 1.9 | % | ISO 62 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
膜刺穿强度Film Puncture Energy | ISO 6603-2 | ||
---- 66 | 2.20 | J | ISO 6603-2 |
---- 77 | 2.60 | J | ISO 6603-2 |
膜刺穿力Film Puncture Force | ISO 6603-2 | ||
---- 66 | 735 | N | ISO 6603-2 |
---- 77 | 838 | N | ISO 6603-2 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
简支梁缺口冲击强度Charpy Notched Impact Strength | ISO 179/1eA | ||
-40℃-40°C | 10 | kJ/m2 | ISO 179/1eA |
-30℃-30°C | 10 | kJ/m2 | ISO 179/1eA |
23℃23°C | 10 | kJ/m2 | ISO 179/1eA |
简支梁无缺口冲击强度Charpy Unnotched Impact Strength | ISO 179/1eU | ||
-30℃-30°C | 60 | kJ/m2 | ISO 179/1eU |
23℃23°C | 75 | kJ/m2 | ISO 179/1eU |
悬臂梁缺口冲击强度Notched Izod Impact Strength | ISO 180/1A | ||
-40℃-40°C | 10 | kJ/m2 | ISO 180-1A |
-30℃-30°C | 10 | kJ/m2 | ISO 180-1A |
悬臂梁无缺口冲击强度Unnotched Izod Impact Strength | ISO 180/1U | ||
-30℃-30°C | 55 | kJ/m2 | ISO 180/1U |
23℃23°C | 65 | kJ/m2 | ISO 180/1U |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
热变形温度热变形温度 | |||
1.8 MPa,未退火1.8 MPa,未退火 | 195 | ℃ | ISO 75-2/A |
0.45 MPa,未退火0.45 MPa,未退火 | 215 | ℃ | ISO 75-2/B |
维卡软化温度Vicat Softening Temperature | |||
B50-- | 210 | ℃ | ISO 306 |
B120-- | 210 | ℃ | ISO 306/B120 |
熔融温度Melting Temperature 55 | 221 | ℃ | ISO 11357-3 |
线性热膨胀系数线性热膨胀系数 | |||
TD:23~55℃TD:23 到 55℃ | 8.0E-5 | 1/℃ | ISO 11359-2 |
MD:23~55℃MD:23 到 55℃ | 3.0E-5 | 1/℃ | ISO 11359-2 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
表面电阻率Surface Resistivity | 1.0E+15 | ohms | IEC 60093 |
体积电阻率体积电阻率 | |||
23℃23℃ | 1.0E+15 | ohms·cm | IEC 60093 |
介电强度介电强度 | |||
23 ℃,1 mm23℃,1.00 mm | 34 | kV/mm | IEC 60243-1 |
相对电容率Relative Permittivity | IEC 60250 | ||
23℃,100 Hz23°C, 100 Hz | 4.30 | IEC 60250 | |
23℃,1 MHz23°C, 1 MHz | 4.00 | IEC 60250 | |
耗散因数Dissipation Factor | IEC 60250 | ||
23℃,100 Hz23°C, 100 Hz | 8.0E-3 | IEC 60250 | |
23℃,1 MHz23°C, 1 MHz | 0.017 | IEC 60250 | |
相比漏电起痕指数Comparative Tracking Index | IEC 60112 | ||
解决方案 ASolution A | 475 | V | IEC 60112 |
解决方案 BSolution B | 225 | V | IEC 60112 |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
阻燃等级Flame Rating | UL 94 | ||
1.60 mm1.6 mm | HB | UL 94 | |
3.20 mm3.2 mm | HB | UL 94 | |
灼热丝可燃性指数灼热丝可燃性指数 | |||
2.0 mm2.0 mm | 600 | ℃ | IEC 60695-2-12 |
极限氧指数Oxygen Index 99 | 23 | % | ISO 4589-2 |
阻燃等级Burning Behavior 1010 | passed | ISO 3795 | |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
ISO ShortnameISO Shortname | PA 6, GHR, 14-100, GF30 | ISO 1874 | |
|
额定值Nominal Value | 单位Units | 测试方法Test Method |
拉伸模量拉伸模量 | |||
23℃23℃ | 10000 | MPa | ISO 527-1-2 |
23℃23℃ | 9910 | MPa | ASTM D638 |
拉伸强度拉伸强度 | |||
断裂,23℃断裂,23℃ | 180 | MPa | ISO 527-2/5 |
断裂,23℃断裂,23℃ | 175 | MPa | ASTM D638 |
拉伸应变拉伸应变 | |||
断裂,23℃断裂,23℃ | 3.0 | % | ISO 527-2/5 |
断裂,23℃断裂,23℃ | 3.0 | % | ASTM D638 |
弯曲模量弯曲模量 | |||
23℃23℃4 | 9300 | MPa | ISO 178-A |
23℃23℃ | 9120 | MPa | ASTM D790 |
弯曲强度Flexural Stress 44 | |||
23℃23℃ | 276 | MPa | ASTM D790 |
3.50% 应变3.5% Strain | -- | MPa | ISO 178-A |
23℃23°C | 270 | MPa | ISO 178 |
弯曲应变Flexural Strain at Flexural Strength 5 (23°C)5 | 4.0 | % | |
球压硬度Ball Indentation Hardness | 230 | MPa | ISO 2039-1 |
江苏普及塑料有限公司
联系人:
何志伟
服务热线:
쌂쌂렉ꠄ렉
쌂쌂렉ꠄ렉
公司地址:
陆家镇陆丰东路3号仕泰隆模具城M区511室
-
注塑级 PP利安德巴塞尔 HP525N 高清晰度 食品接触 易加工 高刚性¥0.01元
-
PP 韩国sk B391G 高抗冲共聚物 高流动 高刚性 食品级 40熔融指数¥0.01元
-
高流动PP 韩国sk/BX3920耐高温高抗冲高刚性注塑级¥0.01元
-
PP 韩国SK B380G 高流动 高抗冲 高光泽 用于家电部件 聚丙烯PP¥0.01元
-
PP韩国SK B330F尺寸稳定高抗撞抗冲共聚物高韧性电池盒电气/电子¥0.01元
-
注塑级 PP/韩国sk/B340F 高强度 高抗冲 共聚物 电子电器¥0.01元
-
PP台湾李长荣6331注塑颗粒低气味新料食品容器瓶盖均聚物塑胶原料¥0.01元
-
PP李长荣化工(福聚)PC366-3瓶盖料单聚合物高强度透明PP料PC366-4¥0.01元
供应PA6/德国朗盛/BKV30GH2.0 900051 热稳定性 玻纤30% 耐老化相关产品
- 专注PA6 玻纤增强30%德国巴斯夫B3W
- 供应PA6 易流动德国朗盛 B30S快速固化
- 供应 注塑 PA6 易流动德国朗盛 B30S PA6 易脱模 快速固化 PA6 尼龙进口塑料
- 专注 PA6 玻纤增强30%德国巴斯夫B3W PA6 尼龙进口塑料 PA6 玻纤增强
- 25%玻纤PA6 DOMAMID 6G25V0EF
- 25%玻纤PA6 DOMAMID 6G25
- 30%玻纤PA6 DOMAMID 6G30
- 30%玻纤PA6 DOMAMID 6G30GT96M
- 30%玻纤PA6 DOMAMID 6G30FC
- 20%玻纤PA6 DOMAMID 6G20GT96M
- PA6 DOMAMID 6G20V0EF
- 30%玻纤PA6 DOMAMID 6G30H
- 供应 防火PA6 广东新会美达 M2800本色耐高温,无卤增强塑料厂家批发价格
- 供应透明 YH800湖南岳化PA6尼龙中粘度塑料原料厂家直销
- 塑胶原料PA6台湾集盛TP-4208高熔子耐低温电子电器专用尼龙PA6纯树脂
- PA6价格塑料美国舒尔曼 6 GF15 流动性耐油性能尼龙塑料颗粒
- 黑色粒子PA6塑胶 美国舒尔曼 GF30润滑剂 导电性PA6塑料颗粒
- 注塑级尼龙塑胶PA6 美国舒尔曼 6MV14 FR4 K1681销售尼龙塑胶原料
猜你在找
- 聚酰胺PA6塑胶原料PA6 美国杜邦 73G30HSL 增强级 工程塑料
- 销售30%矿物填料PA6 基础创新塑料 美国 BG6 注塑级
- 无卤阻燃 塑料原料PA6 日本东丽 CM1007 注塑级工程塑料 低粘度尼龙树脂
- 高流动注塑级PA6纯树脂PA6 日本三菱工程 1010C 注塑级
- 供应注塑级本色纯树脂PA6 日本三菱工程 CM1017 注塑级
- 高刚性PA6 日本三菱工程 1010N2-2 高流动注塑级PA6纯树脂
- 销售尼龙塑料PA6 沙特阿美 P27Z家用电器pA6塑料PA6塑料材料
- 尼龙塑料颗粒PA6 荷兰DSM K-FHGM35高流动性热稳定性PA6塑料
- 聚酰胺树脂PA6 荷兰DSM K-FHGM24矿物增强20%高流动性工程塑料
- 尼龙树脂PA6 荷兰DSM K-FHG7玻纤增强35%尼龙塑胶原料
- 玻纤增强15%PA6尼龙 荷兰DSM K-FHG3高流动性热稳定性PA6塑胶
- 销售尼龙塑料PA6 荷兰DSM K-FHG12玻纤增强热稳定高流动尼龙塑胶
免责声明:以上展示的供应PA6/德国朗盛/BKV30GH2.0 900051 热稳定性 玻纤30% 耐老化信息由江苏普及塑料有限公司自行提供,内容的真实性、准确性和合法性由发布企业负责,
全球塑胶网对此不承担责任。
风险防范建议:为保障您的利益,建议优先选择速购通会员
手机版:供应PA6/德国朗盛/BKV30GH2.0 900051 热稳定性 玻纤30% 耐老化
更新产品链接为:https://www.51pla.com/html/sellinfo/486/48619126.htm
发送询价单